Blog

Peeling: Inter Coat Peeling in Protected Areas

Apr 19, 2023 | Uncategorized

Adhesion is lost under porches or any other protected areas.

Possible Causes:

  • Air pollution or other types of contamination can cause buildup.
  • Salts were not removed before applying the new coat of paint.
  • The new paint is applied to glossy hard films.
  • The surface was not prepared enough.

Solutions:

  • Properly prepare the surface of the area that will be painted.
  • Pay more attention to the areas that are not directly exposed to weathering.
  • Make sure the adhesion is adequate.